The same hot-melt marking paint, the same road surface with different construction teams are likely to have very different marking quality. Some road markings have a 12-month warranty, and some are likely to have a 6-month warranty. Some will fall off within a few days. Although the quality of architectural coatings is critical, construction technology is crucial in the process of road marking construction.


热熔标线涂料


Zhejiang Brothers Road Marking Co., Ltd. will take you to see the reasons for the peeling of the hot-melt marking paint: there is moisture on the ground, the temperature difference is large, the primer is not dry, the primer is not applied, the ground is not cleaned, and the old line The fusion is not stable.


1. Reason: There is water on the ground


External reason: After the ground is dry, the construction will be carried out


Dry or dry the engineering construction ground when necessary


Amplify the front fire of the silo


Reason: big temperature difference


2. Too low ground temperature will cause road markings to fall off


External reason: moderately increase the mold temperature


Increase the front fire of the silo


When necessary, pre-heat the construction ground of the project


Third, the reason: the primer does not dry


The primer (bright oil) is not sprayed evenly, the coating is too thick, the time interval is short, and the primer is not dry, which will cause the road markings to fall off


External principle: The primer is sprayed evenly, and the lines are drawn after drying.


Fourth, the reason: no coating agent


External principle: apply primer evenly


Fifth, the reason: the ground is not cleaned


The ground has dust, sand, oil stains, etc.


External treatment: cleaning and blowing the construction ground of the project


Soil and oil stains should be ground and polished first, and then the construction will be carried out after blowing clean.


Flow, reason: the integration with the old line is not stable


The primer is not applied, the primer is uneven, the primer does not dry, and the old thread is aging


External principle: first polish and polish the old lines, apply primer evenly, and draw lines after the primer dries.

label

0

Recent browsing:

Related products

Relevant news

contact

Address: Hongxingqiao Industrial Park, Changxing County, Zhejiang Province 

Mobile: 13567960712 (manager Li)

Tel: 400-9999-262

Tiktok QR code

Official wechat

  

Zhejiang public network security 33052202000516号